Hastelloy X Pipe

Hastelloy X pipe is made of a high-quality alloy material. It has excellent corrosion resistance, high temperature strength and good processing properties, and is widely used in petroleum, chemical industry, pharmaceuticals, aerospace and other fields.

Hastelloy X pipes have excellent corrosion resistance and can be used for a long time in various corrosive environments. This is because a large number of alloying elements are added to the alloy, such as nickel, chromium, molybdenum, etc. These elements form a dense oxide film on the surface of the alloy, which can effectively resist the erosion of various chemical substances. Hastelloy X pipe has excellent high-temperature strength and can maintain high strength and hardness in high-temperature environments. This is because the alloying elements in the alloy can form strengthening molybdenum, which improves the tensile strength and yield strength of the alloy. Lastly, Hastelloy X has good processing properties and can be used for casting, forging, rolling and other processing processes. During the processing process, the fluidity and plasticity of the alloy are relatively good.

Product Parameters

Product NameHastelloy X Pipe
Outer Diameter Round Pipe: 4mm - 200mm
Square Pipe: 10*10mm - 100*100mm
Rectangular Pipe: 10*20mm - 50*100mm
Wall Thickness0.6mm - 6.0mm
Length1 - 6 meters (Length can be customized)
StandardASTM, AISI, JIS, GB, DIN, EN, etc.
SurfaceBlack, Bright Polished, Rough Turning, Matt Surface Treatment, No.4, BA, etc.
CertificateISO, SGS, BV
Production TechnologyHot Rolling, Cold Rolling

Chemical Composition

C Al Si S Ti Cr Mn Fe Ni Cu
0.1 max 0.15 - 0.60 1.0 max 0.015 max 0.15 - 0.60 19.0 - 23.0 1.5 max 39.5 min 30.0 - 35.0 0.75 max

Mechanical Properties

Tensile Strength (ksi) 0.2% Yield Strength (ksi) Elongation % in 2 inches
75 30 30

Physical Performance

Item Value Temperature (°C)
Density 7.94 g/cm³ Room
Specific Heat 0.11 Kcal/kg·C 21°
Melting Range 1357 - 1385°C -
Modulus of Elasticity 196.5 KN/mm² 20°
Electrical Resistivity 98.9 µΩ·cm 20°
Coefficient of Expansion 14.4 µm/m·°C 20 - 100°
Thermal Conductivity 11.5 W/m·K 20°