Monel K-500 pipe is made of a high-performance nickel-copper alloy that has excellent corrosion resistance and high-temperature strength. It is widely put into use in marine engineering, petrochemical industry, aerospace and other fields.
Monel K-500 alloy is primarily composed of nickel, copper, iron and a small amount of carbon. The nickel content constitutes a large part of the total mass of the alloy, which makes Monel K-500 pipe have good corrosion resistance. In addition, the addition of copper and iron further improves the strength and hardness of Monel K-500 pipes. The chemical composition of Monel K-500 contains relatively low carbon content, which gives the alloy good welding and processing properties. Monel K-500 pipes have excellent physical and mechanical properties. At normal temperature, the alloy has high strength and hardness, as well as good plasticity and toughness. In high-temperature environments, Monel K-500 pipes have good oxidation resistance and creep resistance, which enables the alloy to maintain stable performance in high-temperature and high-pressure environments. In addition, Monel K-500 pipe also has good corrosion resistance and can resist the erosion of a variety of chemical substances.
| Product Name | Monel K-500 Pipe |
|---|---|
| Outer Diameter |
Round Pipe: 4mm - 200mm Square Pipe: 10*10mm - 100*100mm Rectangular Pipe: 10*20mm - 50*100mm |
| Wall Thickness | 0.6mm - 6.0mm |
| Length | 1 - 6 meters (Length can be customized) |
| Standard | ASTM, AISI, JIS, GB, DIN, EN, etc. |
| Surface | Black, Bright Polished, Rough Turning, Matt Surface Treatment, No.4, BA, etc. |
| Certificate | ISO, SGS, BV |
| Production Technology | Hot Rolling, Cold Rolling |
| C | Al | Si | S | Ti | Cr | Mn | Fe | Ni | Cu |
|---|---|---|---|---|---|---|---|---|---|
| 0.1 max | 0.15 - 0.60 | 1.0 max | 0.015 max | 0.15 - 0.60 | 19.0 - 23.0 | 1.5 max | 39.5 min | 30.0 - 35.0 | 0.75 max |
| Tensile Strength (ksi) | 0.2% Yield Strength (ksi) | Elongation % in 2 inches |
|---|---|---|
| 75 | 30 | 30 |
| Item | Value | Temperature (°C) |
|---|---|---|
| Density | 7.94 g/cm³ | Room |
| Specific Heat | 0.11 Kcal/kg·C | 21° |
| Melting Range | 1357 - 1385°C | - |
| Modulus of Elasticity | 196.5 KN/mm² | 20° |
| Electrical Resistivity | 98.9 µΩ·cm | 20° |
| Coefficient of Expansion | 14.4 µm/m·°C | 20 - 100° |
| Thermal Conductivity | 11.5 W/m·K | 20° |