• Da Dong Steel Pipe City, Liaocheng City, Shandong Province
  • Sun - Friday, 08:00 am - 09:00 pm
  • +86 15963195307

Inconel 600 Pipe

Inconel 600 pipe is made of a nickel-based superalloy characterized by excellent heat resistance, corrosion resistance and high strength in environments. This alloy is widely used in the chemical, aerospace, heat treatment and power industries, especially in high-temperature applications that require resistance to oxidizing and reducing environments.

  Inconel 600 alloy is mainly composed of nickel and chromium, with a nickel content of approximately 72% and a chromium content of approximately 14%-17%. In addition, the alloy contains a smaller proportion of iron, as well as trace amounts of silicon, carbon and manganese. This unique chemical composition gives Inconel 600 pipe excellent corrosion resistance and mechanical strength at high temperatures. Inconel 600 alloy has excellent mechanical properties over a wide temperature range and is capable of use at temperatures up to 1093°C (2000°F) without losing good creep and fracture resistance. Its corrosion resistance is particularly remarkable and it is highly resistant to a variety of corrosive media, including seawater, organic acids, and high-temperature and high-pressure steam environments.

Product Parameters

Product NameInconel 600 Pipe
Outer Diameter Round Pipe: 4mm - 200mm
Square Pipe: 10*10mm - 100*100mm
Rectangular Pipe: 10*20mm - 50*100mm
Wall Thickness0.6mm - 6.0mm
Length1 - 6 meters (Length can be customized)
StandardASTM, AISI, JIS, GB, DIN, EN, etc.
SurfaceBlack, Bright Polished, Rough Turning, Matt Surface Treatment, No.4, BA, etc.
CertificateISO, SGS, BV
Production TechnologyHot Rolling, Cold Rolling

Chemical Composition

C Al Si S Ti Cr Mn Fe Ni Cu
0.1 max 0.15 - 0.60 1.0 max 0.015 max 0.15 - 0.60 19.0 - 23.0 1.5 max 39.5 min 30.0 - 35.0 0.75 max

Mechanical Properties

Tensile Strength (ksi) 0.2% Yield Strength (ksi) Elongation % in 2 inches
75 30 30

Physical Performance

Item Value Temperature (°C)
Density 7.94 g/cm³ Room
Specific Heat 0.11 Kcal/kg·C 21°
Melting Range 1357 - 1385°C -
Modulus of Elasticity 196.5 KN/mm² 20°
Electrical Resistivity 98.9 µΩ·cm 20°
Coefficient of Expansion 14.4 µm/m·°C 20 - 100°
Thermal Conductivity 11.5 W/m·K 20°